Rod Size
|
diameter: 3mm above, length: 20mm above
|
Nickel
|
58.0-63.0 %
|
Chromium
|
21.0-25.0 %
|
Iron
|
Bal.
|
Aluminum
|
1.0-1.7 %
|
Carbon
|
0.10 %
|
Manganese
|
1.0 %
|
Sulfur
|
0.015 %
|
Silicon
|
0.50 %
|
Copper
|
1.0 %
|
Density
|
8.11 Mg/m3
|
Melting Range
|
1360-1411 °C
|
Specific Heat, 70°F,
|
448, J/kg-°C
|
Permeability at 200 oersted (15.9 kA/m) at 24°C
|
1.003
|
Curie Temperature °C
|
-196
|
Temperature,°F
|
Electrical Resistivity
ohm-circ mil/f
|
Thermal
Conductivity
Btu-in./ft 2-hr°F
|
Coeff. of
Expansion
10-6 in./in./°F
|
Specific
Heat Btu/lb-°F
|
70
|
710
|
78
|
-
|
0.107
|
200
|
716
|
87
|
7.60
|
0.112
|
400
|
727
|
100
|
8.01
|
0.119
|
600
|
735
|
113
|
8.11
|
0.126
|
800
|
741
|
126
|
8.30
|
0.133
|